Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Mobil Vaprotec Light

Category Fluid , Lubricant
Manufacturer ExxonMobil
Trade Name Mobil Vaprotec
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil Vaprotec Light.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces lightly coated with oil; a liquid phase inhibitor to protect surfaces submerged in oil; and vapor space inhibitors to protect surfaces exposed to oil vapors.Mobil Vaprotec Light is recommended for all applications requiring an ISO Viscosity Grade 32, turbine-quality oil with additional rust protection properties. Operation of systems with oil temperatures above 120°F will deplete the vapor phase inhibitors.
Physical Properties Metric English Comments
Specific Gravity 0.875 g/cc
0.875 g/cc
Viscosity Measurement 95
95
Index
Kinematic Viscosity at 40°C (104°F) 30 cSt
30 cSt
Kinematic Viscosity at 100°C (212°F) 5.3 cSt
5.3 cSt
ASTM Color 1.5
1.5
ASTM D1500
Thermal Properties Metric English Comments
Pour Point -7.00 °C
19.4 °F
Flash Point >= 193 °C
>= 379 °F
ASTM D92
Chemical Properties Metric English Comments
Total Acid Number 0.40
0.40
ASTM D664
Descriptive Properties Value Comments
Demulsibility Time (min) 30
to 0 mL
Rust Prevention, Distilled Water pass
ASTM D665A
Rust Prevention, Synthetic Sea Water pass
ASTM D665B