Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.028 - 0.032 cm/cm
0.028 - 0.032 in/in
ASTM D955
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE)
Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV..
Linear Mold Shrinkage, Flow 0.022 - 0.032 cm/cm
0.022 - 0.032 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE.
Linear Mold Shrinkage, Flow 0.022 - 0.032 cm/cm
0.022 - 0.032 in/in
ASTM D955
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer
Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit..
Linear Mold Shrinkage, Flow 0.022 - 0.032 cm/cm
0.022 - 0.032 in/in
ASTM D955
Elastocon TPE Technologies Elastocon® 2825 Thermoplastic Elastomer
Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and ..