Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.028 - 0.032 cm/cm
0.028 - 0.032 in/in
ASTM D955
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE)
Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV..
Linear Mold Shrinkage, Flow 0.028 cm/cm

@Time 86400 sec
0.028 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Faradex KS003AI Acetal Copolymer (Europe-Africa-Middle East)
LNP* FARADEX* KS003AI is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include; EMI/RFI Shielding, Electrically Conductive.This data was supplied by SAB..
Linear Mold Shrinkage, Flow 0.028 cm/cm
0.028 in/in
SABIC Method
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static.
Linear Mold Shrinkage, Flow 0.028 cm/cm
0.028 in/in
SABIC Method
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East)
LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties
Linear Mold Shrinkage, Flow 0.028 cm/cm
0.028 in/in
SABIC Method
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static.
Linear Mold Shrinkage, Flow 0.028 cm/cm
0.028 in/in
ISO 294-4
DSM EcoPaXX® Q-E7300 PA410-I
Tube Extrusion
Linear Mold Shrinkage, Flow 0.028 cm/cm
0.028 in/in
ISO 294-4
DSM EcoPaXX® Q-X07207 PA410-I
Impact Modified
Linear Mold Shrinkage, Flow 0.028 cm/cm
0.028 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.028 - 0.034 cm/cm

@Thickness 4.00 mm
0.028 - 0.034 in/in

@Thickness 0.157 in
E2P method
Eurostar Star L PA66 D51 PA66, Injection Molded
Star L PA66 D51 is a PTFE Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.028 - 0.034 cm/cm

@Thickness 4.00 mm
0.028 - 0.034 in/in

@Thickness 0.157 in
E2P method
Eurostar Star L POM D74 POM, Injection Molded
Star L POM D74 is a Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.028 cm/cm
0.028 in/in
ISO 294-4
Barlog Plastics KEBAFLEX SG 45 A.1 TPE-S, Shore A45, natural
TPE-SInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Flow 0.028 - 0.035 cm/cm

@Time 86400 sec
0.028 - 0.035 in/in

@Time 24.0 hour
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion