Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm | 0.018 - 0.026 in/in | ASTM D955 |
Kolon SPESIN® KP212VO Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm @Thickness 3.17 mm |
0.018 - 0.026 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 700 TFE 15 High Density Polyethylene (HDPE), PTFE Lubricated |
|||
Linear Mold Shrinkage | 0.015 - 0.026 cm/cm @Thickness 3.17 mm |
0.015 - 0.026 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 800 GB 10 Acetal (POM), Glass Bead |
|||
Linear Mold Shrinkage | 0.015 - 0.026 cm/cm @Thickness 3.17 mm |
0.015 - 0.026 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 800 GB 20 Acetal (POM), Glass Bead |
|||
Linear Mold Shrinkage | 0.017 - 0.026 cm/cm @Thickness 3.17 mm |
0.017 - 0.026 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP PA66 HI BLK Nylon 6/6 (PA), Impact Modified - Heat Stabilized - Value Product |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm | 0.018 - 0.026 in/in | |
Lehmann & Voss LUVOCOM® 80-8318-1 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm | 0.018 - 0.026 in/in | ASTM D955 |
Kolon SPESIN® KP212V0BLK Flame Retardant PBT Compound Resin Flame retardant, BLACKApplications: ConnectorsInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm | 0.018 - 0.026 in/in | |
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm @Thickness 3.20 mm |
0.018 - 0.026 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm @Thickness 3.20 mm |
0.018 - 0.026 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm @Thickness 3.20 mm |
0.018 - 0.026 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.020 - 0.026 cm/cm @Thickness 3.20 mm |
0.020 - 0.026 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 299 H X 72279 A NATURAL Impact-Modified Nylon 6/6 (PA); Impact Modified - ESD Protection |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm @Thickness 3.20 mm |
0.018 - 0.026 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm @Thickness 3.20 mm |
0.018 - 0.026 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm @Thickness 3.20 mm |
0.018 - 0.026 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.015 - 0.026 cm/cm @Thickness 3.17 mm |
0.015 - 0.026 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 1000 HI Polybutylene Terephthalate (PBT), Base Resin - Impact Modified |
|||
Linear Mold Shrinkage | 0.016 - 0.026 cm/cm | 0.016 - 0.026 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2855 Thermoplastic Elastomer Elastocon® 2855 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2855 is FDA compliant and well suited for cons.. |
|||
Linear Mold Shrinkage | 0.022 - 0.026 cm/cm @Thickness 3.20 mm |
0.022 - 0.026 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 2800 D-55A Thermoplastic Polyolefin Elastomer (TEO); Non PBB0/PBBE
(discontinued **) Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |
|||
Linear Mold Shrinkage | 0.023 - 0.026 cm/cm @Thickness 3.17 mm |
0.023 - 0.026 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 4700 TFE 10 SI 2 Polytrimethylene Terephthalate (PTT) PTFE 10% - Silicone 2%
&nb PTFE 10% - Silicone 2%Comments:PTFE LubricatedSilicone LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information pro.. |