Kolon SPESIN® KP212V0BLK Flame Retardant PBT Compound Resin

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Kolon
Trade Name SPESIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon SPESIN® KP212V0BLK Flame Retardant PBT Compound Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, BLACKApplications: ConnectorsInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.060 %
0.060 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.018 - 0.026 cm/cm
0.018 - 0.026 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 11 %
11 %
ASTM D638
Flexural Strength 98.0 MPa
14200 psi
ASTM D790
Flexural Modulus 2.628 GPa
381.2 ksi
ASTM D790
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
ASTM D696
Melting Point 224 °C
435 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.2
3.2
ASTM D150
Dielectric Strength 25.0 kV/mm
635 kV/in
ASTM D149
Arc Resistance 85 sec
85 sec
ASTM D495