Material Notes:
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Linear Mold Shrinkage 0.026 cm/cm
0.026 in/in
MD; ASTM D955
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 33
33
ASTM D785
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Elongation at Yield 44 %
44 %
ASTM D638
Tensile Modulus 0.9501 GPa
137.8 ksi
ASTM D638
Flexural Strength 21.0 MPa
3050 psi
ASTM D790
Flexural Modulus 0.800 GPa
116 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 62.2 °C
144 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.8 °C
109 °F