Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned)
Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl..
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines fl..
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Conditioned)
Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes..
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Dry)
Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved c..
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Dry)
Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes..
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Conditioned)
Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved c..