Material Notes:
Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved cycle times while maintaining excellent properties. It exhibits high strength, rigidity and heat resistance. Surface appearance has been improved, cycle times reduced and creep resistance retained. This heat stabilizer version extends the retention of mechanical properties at elevated temperatures while maintaining excellent chemical resistance to greases, oils and hydrocarbons.Applications: window locks, valve bodies, chair shells, door and window hardware, connectors, switch components, relay parts, terminal blocks, power tool housings, gears, chainsaws, blowers, trimmer housings and automotive housings.Information provided by BASF
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 1.1 %
1.1 %
24 Hours; ASTM D570
1.8 %
1.8 %
50% RH; ASTM D570
6.4 %
6.4 %
Saturation; ASTM D570
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
Processing Properties Metric English Comments
Melt Temperature 270 - 295 °C
518 - 563 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Color BK 102
Commercial Status North America
Copyright © lookpolymers.com All Rights Reserved