Multibase Multi-ABS 3245 FR Flame Retardant ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Multibase
Trade Name Multi-ABS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-ABS 3245 FR Flame Retardant ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955-89
Melt Flow 5.0 g/10 min
5.0 g/10 min
(Condition G) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 38.6 MPa
5600 psi
ASTM D638-95
Elongation at Break 40 %
40 %
ASTM D638-95
Flexural Modulus 2.241 GPa
325.0 ksi
RT; ASTM D-790-95
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256-93a
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
injection molded unannealed; ASTM D-648-95
185 °C
365 °F
injection molded annealed; ASTM D-648-95
195 °C
383 °F
compression molded annealed; ASTM D-648-95
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525-95
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0625 in
UL 94
V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
UL 94
Optical Properties Metric English Comments
Gloss 55 %
55 %
ASTM D2457-90