Physical Properties Metric English Comments
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP
BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac..
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP
BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of ..
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP
SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p..
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP
SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain..
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP
SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel..
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP
SMC 0412 is a premium Class-A SMC for on-line painted conductive exterior body applications on cars. These compounds mould to parts with excellent surface quality and low surface conductivity for e..
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP
SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for ..
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP
SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted ..
Linear Mold Shrinkage -0.000500 - 0.0130 cm/cm
-0.000500 - 0.0130 in/in
Average value: 0.00732 cm/cm Grade Count:22
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..