Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HF0972 is a pelleted high density polyethylene Hexene-1 resin for blow molding.Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and cosmetic containers.Advantages: Excellent stress crack resistance, excellent resistance to most chemicals, outstanding rigidity with high impact strength, high melt strength and moderate die swell.Information provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1000 hour

@Thickness 1.90 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.0748 in,
Temperature 122 °F
slit; ASTM D1693
Base Resin Melt Index 0.10 g/10 min
0.10 g/10 min
I<sub>2</sub>
10 g/10 min
10 g/10 min
I<sub>21</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 36.3 MPa
5260 psi
ASTM D638
Tensile Strength, Yield 30.4 MPa
4410 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Front Barrel Temperature 190 °C
374 °F
Head Temperature 190 °C
374 °F
Users viewing this material also viewed the following: