SGL Carbon Group CF 480 Graphite Filler

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer SGL Carbon Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group CF 480 Graphite Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Graphite filler with good tribologic propertiesInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Bulk Density 0.340 g/cc
0.0123 lb/in³
0.640 g/cc
0.0231 lb/in³
Tap Density
Density 2.23 g/cc
0.0806 lb/in³
Real Density
Particle Size <= 1.0 µm
<= 1.0 µm
1%
<= 8.0 µm
<= 8.0 µm
13%
<= 32 µm
<= 32 µm
57%
<= 64 µm
<= 64 µm
82%
<= 96 µm
<= 96 µm
94%
Specific Surface Area 0.672 m²/g
0.672 m²/g
Blaine
Ash <= 1.0 %
<= 1.0 %
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %