Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 3.20 µm | 3.20 µm | Median (Malvern Laser) |
KaMin KaMin® 100C Kaolin Clay - Calcined Calcined clay with new and unique processing and packaging, designed for applications requiring low moisture, such as 2 component urethanes. Prevents the need to pre-dry the mineral.Industry: Adhesi.. |
|||
Particle Size | 3.20 µm | 3.20 µm | Median (Malvern Laser) |
KaMin KaMin® 70C Kaolin Clay - Calcined High brightness, work-horse calcined kaolin clay, extremely low crystalline silica content.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Flat/Mat.. |
|||
Particle Size | 3.20 µm | 3.20 µm | Median (Malvern Laser) |
KaMin Nylok® 171 Kaolin Clay - Surface Treated Amino silane treated calcined kaolin that reinforces polyamide resin systems.Industry: Rubber & PlasticUses: Non-Black Rubber, Nylon, Thermoset, ThermoplasticInformation provided by KaMin LLC. |
|||
Particle Size | 3.20 µm | 3.20 µm | Median (Malvern Laser) |
KaMin Polyplate® P Kaolin Clay - Delaminated Polyplate® P is a high brightness, delaminated clay intended for use in latex paints, water flexography inks, water-based adhesives or water-based systems where increased hiding, tinting strength.. |
|||
Particle Size | 3.20 µm | 3.20 µm | Median (Malvern Laser) |
KaMin Polyfil® 70 Kaolin Clay - Calcined Calcined clays, such as Polyfil® 70, are brighter than most water-washed clays, offering excellent processing and limited reinforcement. They impart outstanding wet/dry electrical properties due .. |
|||
Particle Size | 3.20 µm | 3.20 µm | Median (Malvern Laser) |
KaMin Polyfil® 80 Kaolin Clay - Calcined Higher brightness, medium particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber GoodsInformation provided by KaMin LLC. |
|||
Particle Size | 3.20 µm | 3.20 µm | Median (Malvern Laser) |
KaMin Polyfil® DL Kaolin Clay - Delaminated Large, platy delaminated clay that reduces gas/vapor permeability, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, MasterBatchInform.. |
|||
Particle Size | 3.20 µm | 3.20 µm | Median (Malvern Laser) |
KaMin Polyfil® WC Kaolin Clay - Calcined Polyfil®WC clay is an organo-functional calcined kaolin clay used in Wire and Cable and other thermoplastic applications. It is designed to reduce water vapor transmission, yields excellent wet a.. |