KaMin Polyfil® 70 Kaolin Clay - Calcined

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Polyfil® 70 Kaolin Clay - Calcined.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Calcined clays, such as Polyfil® 70, are brighter than most water-washed clays, offering excellent processing and limited reinforcement. They impart outstanding wet/dry electrical properties due to the elimination of bound water during the calcined process. Compounds with calcined clays extrude smoothly and reduce stickiness in processing. Polyfil® 70 is a high brightness calcined kaolin clay used to extend elastomeric and thermoplastics products, including wire and cable applications.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, General Plastics, Polyolefins/PVC, Thermoset, Thermoplastic, EPDM, Wire & CableInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.368 - 0.449 g/cc
0.0133 - 0.0162 lb/in³
Loose
Brightness 91 %
91 %
Reflectance (TAPPI)
Oil Absorption 54 %
54 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 0.5 %
<= 0.5 %
As Produced
Particle Size 1.30 µm
1.30 µm
Average Stokes Equivalent Diameter
3.20 µm
3.20 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6
6
100 g/250 ml H2O Slurry
Specific Surface Area 8.00 m²/g
8.00 m²/g
BET
Descriptive Properties Value Comments
Bulking Value 21.9 lb.gal
CAS Number 92704-41-1
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA