Material Notes:
Polyfil®WC clay is an organo-functional calcined kaolin clay used in Wire and Cable and other thermoplastic applications. It is designed to reduce water vapor transmission, yields excellent wet and dry electrical properties, and also long-term stability in EPR and cross-linked polyethylene. Calcined clays have low conductivity due to the elimination of bound water during the calcined process. Compounds with calcined clays extrude smoothly and reduce stickiness in processing.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 91 %
91 %
Reflectance (TAPPI)
Oil Absorption 54 %
54 %
Moisture Absorption at Equilibrium <= 0.5 %
<= 0.5 %
As Produced
Particle Size 1.40 µm
1.40 µm
Average Stokes Equivalent Diameter
3.20 µm
3.20 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.01% Retained
pH 6
6
100 g/250 ml H2O Slurry
Specific Surface Area 7.00 - 9.00 m²/g
7.00 - 9.00 m²/g
BET
Descriptive Properties Value Comments
CAS Number Proprietary
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA