KaMin Nylok® 171 Kaolin Clay - Surface Treated

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Nylok® 171 Kaolin Clay - Surface Treated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amino silane treated calcined kaolin that reinforces polyamide resin systems.Industry: Rubber & PlasticUses: Non-Black Rubber, Nylon, Thermoset, ThermoplasticInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.63 g/cc
2.63 g/cc
Brightness 91 %
91 %
Reflectance (TAPPI)
Moisture Absorption at Equilibrium <= 0.5 %
<= 0.5 %
As Produced
Particle Size 1.40 µm
1.40 µm
Average Stokes Equivalent Diameter
3.20 µm
3.20 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.01% Retained
pH 6
6
100 g/250 ml H2O Slurry; before treatment
8.5
8.5
100 g/250 ml H2O Slurry; after treatment
Descriptive Properties Value Comments
CAS Number Proprietary
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA