Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 6.0 - 10 µm | 6.0 - 10 µm | 10% finer than |
Potters Industries Sphericel® 60P18 Hollow Glass Spheres Description: This microsphere is strong with a density of 0.6g/cc, and has the added advantage of a very small particle size of only 18 micron (mean). Fused glass, hollow spheres used as an additive.. |
|||
Particle Size | 7.0 - 10 µm | 7.0 - 10 µm | mean value |
Potters Industries Spheriglass® 5000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Size | 2.0 - 10 µm | 2.0 - 10 µm | |
Potters Industries Spheriglass® EMB-10 Low Alkaline Boro-Silicate Solid Glass Microspheres Spheriglass® solid glass microspheres have been developed as a filler for paints, coatings, and films.Information provided by Potters Industries. |
|||
Particle Size | 5.0 - 10 µm | 5.0 - 10 µm | d50 |
Magyar Aluminum ALO-DN-7P Alumina Ground Alumina |
|||
Particle Size | 5.0 - 10 µm | 5.0 - 10 µm | d50 |
Magyar Aluminum ALOLT 30AF Aluminum Hydroxide Ground type |
|||
Particle Size | 5.0 - 10 µm | 5.0 - 10 µm | d50 |
Magyar Aluminum ALO-P95-08 Alumina Alumina for Polishing |
|||
Particle Size | 7.0 - 10 µm | 7.0 - 10 µm | Mean particle size is 7 to 10 µm. Crystal size is 4 µm. %-325 mesh is 99.9%. |
Momentive Performance Materials HCP Boron Nitride (BN) Powder Grade HCP is a fine mesh hexagonal Boron Nitride (BN) powder (99%, -325 mesh). It exhibits the unique properties of boron nitride in a form readily used in the production of many advanced materials.. |
|||
Particle Size | 7.0 - 10 µm | 7.0 - 10 µm | Laser Diffraction D50 |
H.C. Starck Grade A Titanium Nitride Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets |
|||
Particle Size | 2.0 - 10 µm | 2.0 - 10 µm | |
American Elements Silver Nanoparticles General DescriptionSilver (Ag) Nanoparticles, nanodots or nanopowder are spherical or flake high surface area metal particles. Nanoscale Silver Particles are typically 1 - 40 nanometers (nm) with sp.. |
|||
Particle Size | 3.0 - 10 µm | 3.0 - 10 µm | Thin Section Crystal Size |
CoorsTek Pure SiC™ HR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
Particle Size | 3.0 - 10 µm | 3.0 - 10 µm | Thin Section Crystal Size |
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
Particle Size | 6.0 - 10 µm | 6.0 - 10 µm | Mean particle size |
Carborundum CarboTherm™ CTF10 Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |
|||
Particle Size | 5.0 - 10 µm | 5.0 - 10 µm | Mean particle size |
Carborundum CarboTherm™ CTF5 Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |