Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 7.0 µm | 7.0 µm | median; Microtrac |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Particle Size | <= 7.0 µm | <= 7.0 µm | 90% smaller than |
Nyco NYAD® 5000 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | >= 7.0 µm | >= 7.0 µm | 10% smaller than |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Particle Size | 7.0 µm | 7.0 µm | Median; Laser Diffraction |
Nabaltec APYRAL® AOH 20 AlO(OH) Boehmite Mineral flame retardant for wire and cable industry, electronic industry and public transport.Properties:High temperature applicationsLow sedimentation at good viscosity performance in resinsGood ch.. |
|||
Particle Size | 7.0 µm | 7.0 µm | 50% of particles, (REG Powder) |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 7.0 µm | 7.0 µm | 50% of particles, (REG Powder) |
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 7.0 - 14 µm | 7.0 - 14 µm | average |
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 7.0 - 14 µm | 7.0 - 14 µm | average |
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 7.0 - 15 µm | 7.0 - 15 µm | average |
Malvern Minerals Novakup® 325 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 7.0 - 11 µm | 7.0 - 11 µm | Mean (agglomerates) |
Momentive Performance Materials AC6003 Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powders of grades HCV, AC6003, and AC6097 are agglomerates composed of submicron hexagonal turbostratic crystals. The mean particle size for these fine powder.. |
|||
Particle Size | 7.0 - 10 µm | 7.0 - 10 µm | Mean particle size is 7 to 10 µm. Crystal size is 4 µm. %-325 mesh is 99.9%. |
Momentive Performance Materials HCP Boron Nitride (BN) Powder Grade HCP is a fine mesh hexagonal Boron Nitride (BN) powder (99%, -325 mesh). It exhibits the unique properties of boron nitride in a form readily used in the production of many advanced materials.. |
|||
Particle Size | 7.0 - 12 µm | 7.0 - 12 µm | 10% |
H.C. Starck Amperit® 250.071 Water Atomized (NiCr 80-20) |
|||
Particle Size | 7.0 - 11 µm | 7.0 - 11 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade AT Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Particle Size | 7.0 µm | 7.0 µm | 50% of particles, (REG Powder) |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 7.0 µm | 7.0 µm | 50% of particles, (REG Powder) |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 7.0 µm | 7.0 µm | 50% of particles, (REG Powder) |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 7.0 µm | 7.0 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 811 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 7.0 µm | 7.0 µm | Before Conversion |
Silberline Aquavet® 651-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline EternaBrite® 651-7 EternaBrite® pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and offer enhanced leafing properties in solvent and waterborn.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline EternaBrite® 651-PA EternaBrite® pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and offer enhanced leafing properties in solvent and waterborn.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline Sparkle Silver® 7000-AR Sparkle Silver® 7000-AR is an super fine, bright non-leafing aluminum pigment with good opacity for solvent-based general industrial coatings. It provides excellent coverage and color.Application.. |
|||
Particle Size | 7.0 µm | 7.0 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 611 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 7.0 µm | 7.0 µm | D50 (Malvern) Size D |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | >= 7.0 µm | >= 7.0 µm | |
Chesterton 787 Sliding Paste Description: Chesterton® 787 Sliding Paste is a premium quality pure synthetic lubricant that will function affectivity even at ultra high temperatures and pressures. Designed for the most severe o.. |
|||
Particle Size | 7.0 µm | 7.0 µm | D90 |
Dandong Taico Minerals TAICOCITE® TC35 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 7.0 - 13 µm | 7.0 - 13 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 3501 EXD Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Asahi Glass Fluon® L173J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
ATI Wah Chang Spectrographic Grade Zirconium Oxide, ZrO2 Spectrographic Grade. A fine, white powder.Information provided by ATI Wah Chang |
|||
Particle Size | 7.0 µm | 7.0 µm | median; Microtrac |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |