Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 0.30 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.30 - 0.50 µm
0.30 - 0.50 µm
Primary
NYC YT3W Y2O3 Powder
Particle Size 0.30 - 0.50 µm
0.30 - 0.50 µm
Primary
NYC YT3WP Y2O3 Granules
Particle Size 0.30 µm
0.30 µm
median
Imerys Aftonâ„¢ Kaolin
Afton is a fine-grained air floating kaolin which is widely used as an anit-caking agent in certain agricultural compounds.Information provided by Imerys
Particle Size 0.30 µm
0.30 µm
median
Imerys Aftonâ„¢ R Kaolin
Afton is a fine-grained kaolin used asa a filler in hard rubber products, plastic products, adhesives, protective coatings and similar applications.Information provided by Imerys
Particle Size 0.30 µm
0.30 µm
median
Imerys Amlockâ„¢ 321 Kaolin
Information provided by Imerys
Particle Size 0.30 µm
0.30 µm
median
Imerys Bardenâ„¢ Kaolin
Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys
Particle Size 0.30 µm
0.30 µm
median
Imerys Bardenâ„¢ R Kaolin
Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys
Particle Size 0.30 µm
0.30 µm
median
Imerys Barnetâ„¢ Kaolin
Information provided by Imerys
Particle Size 0.30 µm
0.30 µm
average
Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin
KT 90A-1 is a Hydraetd Aluminum Silicate. It is a high surface area, fine particle size clay that is well suited for use as an econoMical filler.Information provided by Imerys
Particle Size 0.30 µm
0.30 µm
average
Imerys Kaolexâ„¢ BN Kaolin
Kaolex BN is a Hydrated Aluminum Silicate. It is an econoMical high surface area clay, well suited for use in roofing granules and refractory applications..Information provided by Imerys
Particle Size 0.30 µm
0.30 µm
median
Imerys Mercapâ„¢ 100 Kaolin
Information provided by Imerys
Particle Size 0.30 - 5.0 µm
0.30 - 5.0 µm
TEM
Gwent Electronic Materials P2121112P1 Acid Vapor Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Particle Size 0.30 - 5.0 µm
0.30 - 5.0 µm
TEM
Gwent Electronic Materials P2121112P2 Argon Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Particle Size 0.30 - 5.0 µm
0.30 - 5.0 µm
TEM
Gwent Electronic Materials P2121112P4 Nitrogen Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Particle Size 0.30 - 5.0 µm
0.30 - 5.0 µm
TEM
Gwent Electronic Materials P2121112P5 Ammonia Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Particle Size 0.30 - 5.0 µm
0.30 - 5.0 µm
TEM
Gwent Electronic Materials P2121112P6 Oxygen Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Particle Size 0.30 - 5.0 µm
0.30 - 5.0 µm
TEM
Gwent Electronic Materials P2121112P3 Tetrafluoromethane Plasma Modified Graphene Nanoplatelets
Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd.
Particle Size 0.30 µm
0.30 µm
Shin-Etsu Silicones X-52-2265 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Particle Size 0.30 - 25 µm
0.30 - 25 µm
PSD (d<sub>50</sub>
Terio Corporation TZY-3 Yttria Stabilized Zirconia
Information provided by TERIO Corporation.
Particle Size 0.30 - 0.50 µm
0.30 - 0.50 µm
Planar Size
Goodfellow HDPlas® GNP Plasma Functionalized Graphene Nanoplatelets
Graphene is a carbon based material which is inherently inert and which does not like to mix with, or bond to, other materials. Its excellent properties can only be fully realized when this fundamen..
Particle Size 0.30 - 0.70 µm
0.30 - 0.70 µm
American Elements Titanium Nanoparticles
General DescriptionTitanium (Ti) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Titanium Particles are typically 10 - 80 nanometers (nm) ..
Particle Size 0.30 - 0.60 µm
0.30 - 0.60 µm
MA147LFE
C.O.I.M. FILCO® 368 Film Former for Glass Fiber Sizes
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar..
Particle Size 0.30 µm
0.30 µm
Asahi Glass Fluon® XAD938 PTFE Aqueous Dispersion
Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc...
Particle Size 0.30 µm
0.30 µm
Asahi Glass Fluon® AD936 PTFE Aqueous Dispersion
Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc...
Copyright © lookpolymers.com All Rights Reserved