Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin

Category Ceramic , Clay , Kaolin Clay
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name Hydrated Aluminum Silicate
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys Hydrated Aluminum Silicate KT 90A-1 Kaolin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KT 90A-1 is a Hydraetd Aluminum Silicate. It is a high surface area, fine particle size clay that is well suited for use as an econoMical filler.Information provided by Imerys
Physical Properties Metric English Comments
Brightness 70 - 80 %
70 - 80 %
% Reflectance
Oil Absorption 33 - 38 %
33 - 38 %
g/100g clay; rub out method
Particle Size 0.30 µm
0.30 µm
average
Particle Mesh Size 325 Mesh
325 Mesh
0.1% retained
pH 4.0 - 5.5
4.0 - 5.5
0.28
Specific Surface Area 12 - 15 m²/g
12 - 15 m²/g
Descriptive Properties Value Comments
Color white
Heating Loss (% max as produced) 1
at 105ºC