Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.20 - 0.50 µm | 0.20 - 0.50 µm | outside diameter |
NanoAmor 95%; OD: 200-500 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | 0.30 - 0.50 µm | 0.30 - 0.50 µm | Primary |
NYC YT3W Y2O3 Powder |
|||
Particle Size | 0.20 - 0.50 µm | 0.20 - 0.50 µm | outside diameter |
NanoAmor 95%; OD: 200-500 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Particle Size | 0.30 - 0.50 µm | 0.30 - 0.50 µm | Primary |
NYC YT3WP Y2O3 Granules |
|||
Particle Size | 0.20 - 0.50 µm | 0.20 - 0.50 µm | Crystal Size |
Momentive Performance Materials NX1 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Particle Size | 0.20 - 0.50 µm | 0.20 - 0.50 µm | Crystal Size |
Momentive Performance Materials NX10 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Particle Size | 0.20 - 0.50 µm | 0.20 - 0.50 µm | Crystal Size |
Momentive Performance Materials NX5 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Particle Size | 0.20 - 0.50 µm | 0.20 - 0.50 µm | Crystal Size |
Momentive Performance Materials NX9 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Particle Size | 0.15 - 0.50 µm | 0.15 - 0.50 µm | Dispersed |
Shamrock Technologies NanoFLON® P 47A Thermoplastic Grade PTFE Additive Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro.. |
|||
Particle Size | 0.30 - 0.50 µm | 0.30 - 0.50 µm | Planar Size |
Goodfellow HDPlas® GNP Plasma Functionalized Graphene Nanoplatelets Graphene is a carbon based material which is inherently inert and which does not like to mix with, or bond to, other materials. Its excellent properties can only be fully realized when this fundamen.. |
|||
Particle Size | 0.10 - 0.50 µm | 0.10 - 0.50 µm | SiC Crystal Size |
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |
|||
Particle Size | 0.25 - 0.50 µm | 0.25 - 0.50 µm | MA147LFE |
C.O.I.M. FILCO® 309 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Particle Size | 0.25 - 0.50 µm | 0.25 - 0.50 µm | MA147LFE |
C.O.I.M. FILCO® 339 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Particle Size | 0.20 - 0.50 µm | 0.20 - 0.50 µm | MA147LFE |
C.O.I.M. FILCO® 362 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |