Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.35 - 2.45 g/cc | 0.0849 - 0.0885 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 150 GM Dense Refractory Castable Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro.. |
|||
Bulk Density | 2.35 - 2.45 g/cc | 0.0849 - 0.0885 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 HS Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc.. |
|||
Bulk Density | 2.35 g/cc | 0.0849 lb/in³ | |
Sharadaa Ceramics LI SILL-II High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | >= 2.35 g/cc | >= 0.0849 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Bulk Density | 2.35 g/cc | 0.0849 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics Smart Cast 9 Medium Cement Castables Information provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 2.35 g/cc | 0.0851 lb/in³ | Packed |
Excalibar NewWate™ Barite BaSO4 Powder NewWate™ barite is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas exploration. NewWate.. |
|||
Bulk Density | 2.35 g/cc | 0.0849 lb/in³ | |
Chosun Refractories COD-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.35 g/cc | 0.0849 lb/in³ | |
Chosun Refractories MSC-1 Blast Furnace Tap-Hole Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.35 g/cc | 0.0849 lb/in³ | |
Chosun Refractories PCB-50 Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |