Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories MSC-1 Blast Furnace Tap-Hole Refractory

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories MSC-1 Blast Furnace Tap-Hole Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.35 g/cc
0.0849 lb/in³
Porosity 28 %
28 %
Mechanical Properties Metric English Comments
Compressive Strength 9.41 MPa

@Temperature 1350 °C,
Time 10800 sec
1370 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage -0.0600 %

@Temperature 1350 °C,
Time 10800 sec
-0.0600 %

@Temperature 2460 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 51 %
51 %
Descriptive Properties Value Comments
Chemical Analysis(%),Si3N4 9
Chemical Analysis(%),SiC+C 23
Main Applications Corex