Chosun Refractories COD-1 Special brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories COD-1 Special brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.35 g/cc
0.0849 lb/in³
Porosity 17 %
17 %
Mechanical Properties Metric English Comments
Compressive Strength 49.0 MPa
7110 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 4.00 µm/m-°C

@Temperature 1000 °C
2.22 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 52 %
52 %
MgO 2.0 %
2.0 %
Descriptive Properties Value Comments
Refractories Under Load(2kg/?,T2?) 1,430
Refractoriness (SK) 35