Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.44 g/cc | 0.0521 lb/in³ | Untapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 3000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Bulk Density | 1.44 g/cc | 0.0520 lb/in³ | |
Reade Advanced Materials Colemanite Powder (2CaO·3Ba2O3·5H V2O) Description: Commonly in distinct crystals, and sometimes thin and platy. Brittle. Transparent. Actively mined in Turkey.Form Available: 70 mesh USS by down.Information provided by Reade Advanced Ma.. |
|||
Bulk Density | 1.44 g/cc | 0.0521 lb/in³ | |
Imerys G-20 HP Feldspar G-20 HP Feldspar is a high potassium aluminium silicate ground to 200 mesh for ceramic applications. G-20HP offers high potassium content and low iron oxide per unit of alumina.Information provided .. |
|||
Bulk Density | 1.44 g/cc | 0.0521 lb/in³ | |
Imerys G-40 HP Feldspar G-40 HP fledpsar is a high potassium aluminium silicate ground to 200 mesh for ceramic applications. G-40 HP offers high potassium content and low iron oxide per unit of alumina.Information provided.. |
|||
Bulk Density | 1.44 g/cc | 0.0521 lb/in³ | Loose |
Excalibar ExBar™ W 400 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Bulk Density | 1.44 - 1.54 g/cc | 0.0520 - 0.0556 lb/in³ | |
3M #11 Roofing Granule (Little Rock) 3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre.. |
|||
Bulk Density | 1.44 - 1.54 g/cc | 0.0520 - 0.0556 lb/in³ | |
3M 7000 Series Copper Roofing Granule (Little Rock) 3M Copper Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and treate.. |
|||
Bulk Density | 1.44 - 1.54 g/cc | 0.0520 - 0.0556 lb/in³ | |
3M Blended #11 Blended Roofing Granule (Little Rock) 3M #11 Grade Blended Roofing Granules are combination of ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a.. |
|||
Bulk Density | 1.44 - 1.54 g/cc | 0.0520 - 0.0556 lb/in³ | |
3M Headlap Roofing Granule (Little Rock) 3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He.. |
|||
Bulk Density | 1.44 g/cc | 0.0520 lb/in³ | Powder |
Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia Two-part, quick-set ceramic for small parts. |
|||
Bulk Density | 1.44 g/cc | 0.0520 lb/in³ | Powder |
Aremco Ceramacast™ 673 Castable Ceramic Chemical setting. Two-part ceramic exhibiting high thermal conductivity. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" de.. |
|||
Bulk Density | 1.44 g/cc | 0.0520 lb/in³ | Powder |
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina Fine grain castable ceramic. |
|||
Bulk Density | 1.44 g/cc | 0.0520 lb/in³ | Powder |
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils .. |