Physical Properties Metric English Comments
Bulk Density 1.44 g/cc
0.0520 lb/in³
Reade Advanced Materials Colemanite Powder (2CaO·3Ba2O3·5H V2O)
Description: Commonly in distinct crystals, and sometimes thin and platy. Brittle. Transparent. Actively mined in Turkey.Form Available: 70 mesh USS by down.Information provided by Reade Advanced Ma..
Bulk Density 1.44 - 1.54 g/cc
0.0520 - 0.0556 lb/in³
3M #11 Roofing Granule (Little Rock)
3M #11 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and tre..
Bulk Density 1.44 - 1.54 g/cc
0.0520 - 0.0556 lb/in³
3M 7000 Series Copper Roofing Granule (Little Rock)
3M Copper Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a ceramic matrix and treate..
Bulk Density 1.44 - 1.54 g/cc
0.0520 - 0.0556 lb/in³
3M Blended #11 Blended Roofing Granule (Little Rock)
3M #11 Grade Blended Roofing Granules are combination of ceramic-coated minerals used as surfacing material in asphalt roofing products. These granules are colored with durable pigments, bonded in a..
Bulk Density 1.44 - 1.54 g/cc
0.0520 - 0.0556 lb/in³
3M Headlap Roofing Granule (Little Rock)
3M Headlap Roofing Granules are ceramic-coated or natural minerals used as headlap surfacing material in asphalt roofing products. These granules are treated to promote adhesion to asphalt. These He..
Bulk Density 1.44 g/cc
0.0520 lb/in³
Powder
Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia
Two-part, quick-set ceramic for small parts.
Bulk Density 1.44 g/cc
0.0520 lb/in³
Powder
Aremco Ceramacast™ 673 Castable Ceramic
Chemical setting. Two-part ceramic exhibiting high thermal conductivity. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" de..
Bulk Density 1.44 g/cc
0.0520 lb/in³
Powder
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina
Fine grain castable ceramic.
Bulk Density 1.44 g/cc
0.0520 lb/in³
Powder
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound
Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils ..