Imerys G-40 HP Feldspar

Category Ceramic , Clay , Feldspar Clay , Oxide , Silicon Oxide
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys G-40 HP Feldspar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
G-40 HP fledpsar is a high potassium aluminium silicate ground to 200 mesh for ceramic applications. G-40 HP offers high potassium content and low iron oxide per unit of alumina.Information provided by Imerys
Physical Properties Metric English Comments
Bulk Density 1.44 g/cc
0.0521 lb/in³
Particle Mesh Size 30 Mesh
30 Mesh
0% retained
40 Mesh
40 Mesh
0.3% retained
200 Mesh
200 Mesh
94.8% retained
Component Elements Properties Metric English Comments
Al2O3 18.2 %
18.2 %
CaO 0.75 %
0.75 %
Fe2O3 0.090 %
0.090 %
K2O 13.2 %
13.2 %
Loss on Ignition(%) 0.16 %
0.16 %
Na2O 1.52 %
1.52 %
SiO2 65.9 %
65.9 %