BASF Neopor® 5300 Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer BASF
Trade Name Neopor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Neopor® 5300 Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a considerably higher thermal-insulation capacity than the usual EPS insulating materials.Applications: Block and molded parts.Information provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
Density 0.00310 g/cc
0.000112 lb/in³
Vapor (Heavier than air)
1.02 - 1.05 g/cc
0.0368 - 0.0379 lb/in³
Bead Size 0.900 - 1.30 mm
0.0354 - 0.0512 in
Thermal Properties Metric English Comments
Softening Point 70.0 °C
158 °F
approx
Decomposition Temperature >= 220 °C
>= 428 °F
Flash Point >= -56.0 °C
>= -68.8 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Color Black
Commercial Status Europe
Ignition Temperature 285°C
DIN 51794
Sieve Analysis <0.8 mm
max 2%
>1.4 mm
max 3%
0.8 - 1.4 mm
max 95%