Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories CSN-A116 Plate Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CSN-A116 Plate Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.15 - 3.25 g/cc
0.114 - 0.117 lb/in³
Porosity 6.0 - 9.0 %
6.0 - 9.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.012753 GPa

@Temperature 1400 °C
<= 1.8497 ksi

@Temperature 2550 °F
Compressive Strength <= 98.1 MPa
<= 14200 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 9.00 - 11.0 µm/m-°C

@Temperature 1000 °C
5.00 - 6.11 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 92 - 96 %
92 - 96 %
Carbon, C 2.0 - 4.0 %
2.0 - 4.0 %
Descriptive Properties Value Comments
Remarks Excellent for high 0 steel, Excellent corrosion resistance
Copyright © lookpolymers.com All Rights Reserved