Physical Properties Metric English Comments
Bulk Density 1.40 g/cc
0.0506 lb/in³
Loose
Nyco HARRP™ 20 X 40 Wollastonite
HARRP™ 20X40 is suggested for concrete and concrete roof tile reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive..
Bulk Density 1.40 - 1.60 g/cc
0.0506 - 0.0578 lb/in³
JIS K5101
NYC YT3WBHQ Y2O3 Powder for Spray Coating
High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.Narrow particle size distributionTailorable for each spray coating technologyNo c..
Bulk Density 1.40 g/cc
0.0506 lb/in³
Tap Density of Granules
NYC YT3WBQ Y2O3 CIP (Cold Isostatic Pressing) Granules
99.9% and better high purity granules produce high quality finished ceramics. Uses include semiconductors / LCD industries, metallurgy, magnets, and electroceramics.Acrylic binder systemExcellent g..
Bulk Density 1.40 g/cc
0.0506 lb/in³
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation
Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos..
Bulk Density <= 1.40 g/cc
<= 0.0506 lb/in³
Magyar Aluminum ALOLT 01 Aluminum Hydroxide
Dry type
Bulk Density 1.40 g/cc
0.0506 lb/in³
MarkeTech Repton 931 Cordierite Mg-Al-Si Oxide
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
Bulk Density 1.40 g/cc
0.0506 lb/in³
Tap Density; ASTM B527
H.C. Starck FeCoCu Prealloyed Metal Powder
A new prealloyed metallic powder of high sinter-activity with ideally homogenized constituents at an atomic level. The primary particles of very fine grain size are loosely agglomerated to agglomera..
Bulk Density 1.40 - 1.50 g/cc
0.0506 - 0.0542 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable
Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p..
Bulk Density 1.40 - 1.50 g/cc
0.0506 - 0.0542 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable
Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al..
Bulk Density 1.40 g/cc

@Temperature 200 °C
0.0506 lb/in³

@Temperature 392 °F
Sharadaa Ceramics Sharada LTM 1.4 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Bulk Density 1.40 g/cc
0.0506 lb/in³
Size B (tapped)
Vesta Ceramics SicoMill® Grade 2 Silicon Powder
General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu..
Bulk Density 1.40 g/cc
0.0506 lb/in³
Size B (tapped)
Vesta Ceramics SicoMill® Grade 4 Silicon Powder
General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu..
Bulk Density 1.40 g/cc
0.0506 lb/in³
Zircar Zirconia FBD Zirconia Boards, Discs, and Cylinders Insulation
Type FBD Boards, Discs and Cylinders are high strength, uniform, rigid, refractory structures composed of zirconia fibers stabilized with yttria. Type FBD is Zircar Zirconia's strongest and mos..
Bulk Density 1.40 - 1.50 g/cc
0.0506 - 0.0542 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable
Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema..