Gouda Vuurvast GOLITE 180 Refractory Insulating Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name GOLITE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast GOLITE 180 Refractory Insulating Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.40 - 1.50 g/cc
0.0506 - 0.0542 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 13.0 - 17.0 MPa

@Temperature 1500 °C
1890 - 2470 psi

@Temperature 2730 °F
Cold Crushing Strength
14.0 - 18.0 MPa

@Temperature 100 °C
2030 - 2610 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.780 - 0.880 W/m-K

@Temperature 1500 °C
5.41 - 6.11 BTU-in/hr-ft²-°F

@Temperature 2730 °F
1.22 - 1.42 W/m-K

@Temperature 600 °C
8.47 - 9.85 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.80 - 2.20 W/m-K

@Temperature 100 °C
12.5 - 15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1800 °C
3270 °F
Shrinkage -0.300 - 0.500 %

@Temperature 1500 °C
-0.300 - 0.500 %

@Temperature 2730 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 94 %
94 %
Fe2O3 <= 0.20 %
<= 0.20 %
SiO2 <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
ASTM Classification V
Material Consumption per 1 m3 1400 kg
Mixing Water 17-22 liters
per 100 kgs dry material