Polymer Property : Linear Mold Shrinkage, Transverse = 0.019 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm

@Time 86400 sec
0.017 - 0.019 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12
LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm

@Time 86400 sec
0.017 - 0.019 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm

@Time 86400 sec
0.017 - 0.019 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer
LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm

@Time 86400 sec
0.017 - 0.019 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific)
LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications.