SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
1.18 g/cc
0.0426 lb/in³
ISO 1183
Moisture Absorption 0.100 %
0.100 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.017 - 0.019 cm/cm

@Time 86400 sec
0.017 - 0.019 in/in

@Time 24.0 hour
ASTM D955
0.018 cm/cm

@Time 86400 sec
0.018 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.017 - 0.019 cm/cm

@Time 86400 sec
0.017 - 0.019 in/in

@Time 24.0 hour
ASTM D955
0.018 cm/cm

@Time 86400 sec
0.018 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.0 MPa
6820 psi
ASTM D638
49.0 MPa
7110 psi
ISO 527
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM D638
49.0 MPa
7110 psi
ISO 527
Elongation at Break 14.3 %
14.3 %
ASTM D638
15.6 %
15.6 %
ISO 527
Elongation at Yield 13.6 %
13.6 %
ASTM D638
15.2 %
15.2 %
ISO 527
Tensile Modulus 2.06 GPa
299 ksi
50 mm/min; ASTM D638
2.19 GPa
318 ksi
1 mm/min; ISO 527
Flexural Strength 65.0 MPa
9430 psi
ISO 178
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
2.06 GPa
299 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.71 J/cm
10.7 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 39.0 kJ/m²
18.6 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 J
2.21 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Coefficient of Friction, Dynamic 0.24
0.24
ASTM D3702 Modified
Coefficient of Friction, Static 0.27
0.27
ASTM D3702 Modified
K (wear) Factor 36.3 x 10-8 mm³/N-M
18.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
157 °C

@Thickness 3.20 mm
315 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
61.0 °C

@Thickness 3.20 mm
142 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: