Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wetting and bonding. In brazing gray cast iron it is necessary to treat the surface prior to brazing to remove graphite, in order to assure good wetting by the brazing filler metal. A complete list of the uses of Easy-Flo would include practically all applications for which silver brazing filler metals have been used. Characteristics:Easy-Flo is a are eutectic type, free-flowing filler metals that, because of their narrow melting range, are less sensitive to the rate of heating and should not liquate (i.e. separate into low and high melting constituents). This high fluidity makes well-fitted joints essential and prevents bridging or large fillet formation. Handy Flux should be used with either of these filler metals.Some base metals when brazed under high stress may crack during brazing when the stressed base metal is wetted by the brazing filler metal. This is a form of stress corrosion cracking. The low flow temperature of Easy-Flo is below the stress relaxation temperature of some nickel base alloys. The cure is to relieve the stress before the brazing alloy is applied. A higher melting brazing filler metal may be preferred since stress relief will then occur before the filler metal melts. Specifications:This filler metal conform to the following specifications: AWS A5.8 BAg-1a, SAE-AMS 4770, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-1a Information provided by Lucas-Milhaupt, Inc.
Physical Properties Metric English Comments
Density 9.45 g/cc
0.341 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 379 MPa
55000 psi
Armco Iron (0.05% C) butt joint
414 MPa
60000 psi
Stainless Steel (18-8) Annealed butt joint
448 MPa
65000 psi
1020 Steel butt joint
586 MPa
85000 psi
1095 (Drill Rod) butt joint
621 MPa
90000 psi
High Speed Steel (18 W, 4 Cr, 1 V) butt joint
758 MPa
110000 psi
4140 Steel butt joint
896 MPa
130000 psi
Stainless Steel 918-8) Cold Rolled butt joint
55.2 MPa

@Temperature 482 °C
8000 psi

@Temperature 900 °F
Inconel butt joint
82.7 MPa

@Temperature 427 °C
12000 psi

@Temperature 800 °F
Stainless Steel (18-8) butt joint
89.6 MPa

@Temperature 482 °C
13000 psi

@Temperature 900 °F
Monel butt joint
262 MPa

@Temperature 260 °C
38000 psi

@Temperature 500 °F
Inconel butt joint
310 MPa

@Temperature 23.0 °C
45000 psi

@Temperature 73.4 °F
331 MPa

@Temperature 260 °C
48000 psi

@Temperature 500 °F
Monel butt joint
338 MPa

@Temperature 260 °C
49000 psi

@Temperature 500 °F
Stainless Steel (18-8) butt joint
483 MPa

@Temperature 23.0 °C
70000 psi

@Temperature 73.4 °F
696 MPa

@Temperature 23.0 °C
101000 psi

@Temperature 73.4 °F
Elongation at Break 0.00 %

@Temperature 260 °C
0.00 %

@Temperature 500 °F
in 2", Stainless Steel (18-8) butt joint
0.00 %

@Temperature 260 °C
0.00 %

@Temperature 500 °F
in 2", Inconel butt joint
0.00 %

@Temperature 427 °C
0.00 %

@Temperature 800 °F
in 2", Stainless Steel (18-8) butt joint
0.00 %

@Temperature 482 °C
0.00 %

@Temperature 900 °F
in 2", Inconel butt joint
0.00 %

@Temperature 482 °C
0.00 %

@Temperature 900 °F
in 2", Monel butt joint
0.00 %

@Temperature 23.0 °C
0.00 %

@Temperature 73.4 °F
0.00 %

@Temperature 23.0 °C
0.00 %

@Temperature 73.4 °F
3.1 %

@Temperature 260 °C
3.1 %

@Temperature 500 °F
in 2", Monel butt joint
7.3 %

@Temperature 23.0 °C
7.3 %

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 627 - 635.0 °C
1160 - 1175 °F
Solidus 627 °C
1160 °F
Melting Point
Liquidus 635.0 °C
1175 °F
Flow Point
Component Elements Properties Metric English Comments
Cadmium, Cd 17 - 19 %
17 - 19 %
Copper, Cu 14.5 - 16.5 %
14.5 - 16.5 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 49 - 51 %
49 - 51 %
Zinc, Zn 14.5 - 18.5 %
14.5 - 18.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000700 ohm-cm
0.00000700 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 635.0 - 746.1 °C
1175 - 1375 °F
Brazing Range
Descriptive Properties Value Comments
Color Light Yellow