Polymer Property : Density = 8.87 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.87 g/cc
0.320 lb/in³
Indium Corp. Indalloy 116 Tin-Lead Solder Alloy
General purpose solderInformation Provided by Indium Corporation
Density 8.87 g/cc
0.320 lb/in³
Williams Advanced Alloys WS212 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TB00 Solution HT
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TD01 1/4 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TD02 1/2 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TD03 3/4 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TD04 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TM02
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TM04
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TM06
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TS01
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TS02
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TS03
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TS04
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TX00
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TM00
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Ametek AM 388™ Alloy (UNS C72650) TM08
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Density 8.87 g/cc
0.320 lb/in³
Indium Corp. Indalloy 208 Copper Solder Alloy
Information Provided by Indium Corporation