Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy 208 Copper Solder Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 208 Copper Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.87 g/cc
0.320 lb/in³
Thermal Properties Metric English Comments
Melting Point 665 - 985 °C
1230 - 1810 °F
Solidus 665 °C
1230 °F
Liquidus 985 °C
1810 °F
Component Elements Properties Metric English Comments
Copper, Cu 85 %
85 %
Silver, Ag 7.0 %
7.0 %
Tin, Sn 8.0 %
8.0 %
Users viewing this material also viewed the following: