Physical Properties Metric English Comments
Density 5.60 g/cc
0.202 lb/in³
NanoScale NanoActive® Zinc Oxide
NanoActive ZnO is produced using proprietary processes to obtain high specific surface area, small crystallite size material that can be dispersed in various carrier fluids with significantly reduce..
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Indium Corp. NanoFoil® High Temperature Nickel and Aluminum Sacrificial Heat Source
As a sacrificial heat source in soldering and brazing applications, NanoFoil® is ideal for high-temperature applications. NanoFoil becomes a non-functional part of the solder or braze joint, eli..
Density 5.60 g/cc
0.202 lb/in³
Ferro CF 1417 Low-Temperature Sealing
VITREOUS Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ther..
Density 5.60 g/cc
0.202 lb/in³
American Elements Z-MITE™ Zinc Oxide Nanopowder
General DescriptionZ-MITE powders are inorganic zinc-oxide nanoparticles with antibacterial, antifungal, anti-corrosion, catalytic, and UV filtering properties. Z-MITE-A products are uncoated and hy..
Density 5.60 g/cc
0.202 lb/in³
ASTM-C 20
CoorsTek ZDY Yttria Fully Stabilized Zirconia
Oxygen ionic conductor for high-stress and high-thermal-shock environments
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Alliance BCN-11 Bonded (Composite) Magnetic Material
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Alliance BCN-13 Bonded (Composite) Magnetic Material
Density 5.60 g/cc
0.202 lb/in³
BASF Sicopal® Yellow L 1100 Color Additive
Description: Weather-resistant inorganic bismuth vanadate pigment with high hiding power Chemical Structure: Bismuth vanadatSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems..
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Alliance BCN-10 Bonded (Composite) Magnetic Material
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Alliance BCN-12 Bonded (Composite) Magnetic Material
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Alliance BCN-14 Bonded (Composite) Magnetic Material
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Alliance BCN-15 Bonded (Composite) Magnetic Material
Density 5.60 - 6.00 g/cc
0.202 - 0.217 lb/in³
Alliance BCN-17 Bonded (Composite) Magnetic Material