Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.60 g/cc | 0.202 lb/in³ | |
NanoScale NanoActive® Zinc Oxide NanoActive ZnO is produced using proprietary processes to obtain high specific surface area, small crystallite size material that can be dispersed in various carrier fluids with significantly reduce.. |
|||
Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ | |
Indium Corp. NanoFoil® High Temperature Nickel and Aluminum Sacrificial Heat Source As a sacrificial heat source in soldering and brazing applications, NanoFoil® is ideal for high-temperature applications. NanoFoil becomes a non-functional part of the solder or braze joint, eli.. |
|||
Density | 5.60 g/cc | 0.202 lb/in³ | |
Ferro CF 1417 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ther.. |
|||
Density | 5.60 g/cc | 0.202 lb/in³ | |
American Elements Z-MITE™ Zinc Oxide Nanopowder General DescriptionZ-MITE powders are inorganic zinc-oxide nanoparticles with antibacterial, antifungal, anti-corrosion, catalytic, and UV filtering properties. Z-MITE-A products are uncoated and hy.. |
|||
Density | 5.60 g/cc | 0.202 lb/in³ | ASTM-C 20 |
CoorsTek ZDY Yttria Fully Stabilized Zirconia Oxygen ionic conductor for high-stress and high-thermal-shock environments |
|||
Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ | |
Alliance BCN-11 Bonded (Composite) Magnetic Material |
|||
Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ | |
Alliance BCN-13 Bonded (Composite) Magnetic Material |
|||
Density | 5.60 g/cc | 0.202 lb/in³ | |
BASF Sicopal® Yellow L 1100 Color Additive Description: Weather-resistant inorganic bismuth vanadate pigment with high hiding power Chemical Structure: Bismuth vanadatSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems.. |
|||
Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ | |
Alliance BCN-10 Bonded (Composite) Magnetic Material |
|||
Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ | |
Alliance BCN-12 Bonded (Composite) Magnetic Material |
|||
Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ | |
Alliance BCN-14 Bonded (Composite) Magnetic Material |
|||
Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ | |
Alliance BCN-15 Bonded (Composite) Magnetic Material |
|||
Density | 5.60 - 6.00 g/cc | 0.202 - 0.217 lb/in³ | |
Alliance BCN-17 Bonded (Composite) Magnetic Material |