Polymer Property : Density = 2.46 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.46 g/cc
0.0889 lb/in³
LATI Latigray 62-01 CX/75 PA 6
Radiopaque compound based on Polyamide 6 (PA6). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Density 2.46 g/cc
0.0889 lb/in³
AGY ZenTron® S-2 Generic S-Glass Fiber
S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod..