Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.46 g/cc | 0.0889 lb/in³ | |
LATI Latigray 62-01 CX/75 PA 6 Radiopaque compound based on Polyamide 6 (PA6). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Density | 2.46 g/cc | 0.0889 lb/in³ | |
AGY ZenTron® S-2 Generic S-Glass Fiber S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod.. |