Physical Properties Metric English Comments
Density 1.98 g/cc
0.0715 lb/in³
Cookson Group Plaskon® 1031 Conventional Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, conventional molding compound recommended for high volume commodity-type packages that house simple linear and discre..
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
3M Dyneon™ CC085 PTFE, PPS-Filled  (discontinued **)
Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon.
Density 1.98 g/cc
0.0715 lb/in³
3M Dyneon™ THV™ 500 Fluorothermoplastic  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf..
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Glastic BMC SLC-1000 Glass-Reinforced Polyester
Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage.
Density 1.98 g/cc
0.0715 lb/in³
Meilian Chemical W90218 WHITE MASTERBATCH
WHITE W90218 is a white low density polyethylene based masterbatch containing premium TiO2 and calcium carbonate filler without any content of fluorescence whitener. This product is designed for use..
Density 1.98 g/cc
0.0715 lb/in³
Meilian Chemical W9350 WHITE MASTERBATCH
W9350 is a LDPE based masterbatch designed for use in film products for general purpose.Method of Usage: W9350 is designed for ease of dispersion and is therefore suitable for direct addition and mi..
Density 1.98 g/cc
0.0715 lb/in³
ASTM D572
Haysite H258 Polyester Laminate
Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications..
Density 1.98 g/cc
0.0715 lb/in³
ASTM D572
Haysite H260 Polyester Laminate
Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m..
Density 1.98 g/cc
0.0715 lb/in³
Mateck Potassium Chloride (KCl)
Optical crystals
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® AD 40H Perfluoropolymer
Hyflon® AD 40H is an amorphous perfluoro-polymer available in powder form. Hyflon® AD polymers resemble semicrystalline perfluoropolymers in their performance properties as they exhibit high t..
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® AD 40L Perfluoropolymer
Hyflon® AD 40L is an amorphous perfluoro-polymer available in powder form. Hyflon® AD polymers resemble semicrystalline perfluoropolymers in their performance properties as they exhibit high t..
Density 1.98 g/cc
0.0715 lb/in³
Relative Density; ASTM D792
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy
Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group
Density 1.98 g/cc
0.0715 lb/in³
Relative Density; ASTM D792
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy
Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B..
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Sumitomo Bakelite North America Epiall® 1908B-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided ..
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Westlake Plastics Clariflex® TFE/VF2/HFP
Clariflex is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoro-propylene, and vinylidene fluoride. Notable properties include light transmission, chemical resistance..
Density 1.98 g/cc
0.0715 lb/in³
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica
Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C)
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Sumitomo Bakelite North America Epiall® 1908M-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908M-1 is a short glass fiber reinforced epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information provided..