Material Notes:
Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
value after 15 sec; ASTM D2240
70
70
initial value; ASTM D2240
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D4745
Elongation at Break 170 %
170 %
ASTM D4894
Compressive Yield Strength 9.30 MPa
1350 psi
ASTM D695
Compressive Modulus 0.520 GPa
75.4 ksi
ASTM D695
Coefficient of Friction, Dynamic 0.32
0.32
ASTM D3702
K (wear) Factor 29.4 x 10-8 mm³/N-M
14.6 x 10-10 in³-min/ft-lb-hr
at 5000 psi - fpm PV; ASTM D3702