Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Meilian Chemical W9350 WHITE MASTERBATCH

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Meilian Chemical Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meilian Chemical W9350 WHITE MASTERBATCH.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
W9350 is a LDPE based masterbatch designed for use in film products for general purpose.Method of Usage: W9350 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, free from pollution problem caused by pigment.Range of Application: W9350 is designed for applications of injection molding, blow film and legging in LDPE, HDPE, LLDPE, and PP.
Physical Properties Metric English Comments
Density 1.98 g/cc
0.0715 lb/in³
Melt Index of Compound 15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Carrier LDPE
Compatibility LDPE, HDPE, PP and Ethylene copolymer
Pigment Content: TiO2 (%) 47
Users viewing this material also viewed the following: