Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastic Armlen® PP GF 30-5HS-901 Polypropylene, 30% Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Polyplastic Group
Trade Name Armlen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armlen® PP GF 30-5HS-901 Polypropylene, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat stabilized, black colorInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ISO 527
Flexural Modulus 5.60 GPa
812 ksi
ISO 178
Izod Impact, Unnotched (ISO) 50.0 kJ/m²

@Temperature -45.0 °C
23.8 ft-lb/in²

@Temperature -49.0 °F
ISO 180/1eA
54.0 kJ/m²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
ISO 75A
Processing Properties Metric English Comments
Melt Temperature 145 °C
293 °F
Mold Temperature 60.0 °C
140 °F
Drying Temperature 85.0 °C

@Time 3600 - 7200 sec
185 °F

@Time 1.00 - 2.00 hour