Polymer Property : Density = 1.111 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.111 g/cc
0.04014 lb/in³
ISO 1183
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66
PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS.
Density 1.111 g/cc
0.04014 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS
LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber.
Density 1.111 g/cc
0.04014 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS
LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber.
Density 1.111 g/cc
0.04014 lb/in³
ASTM D792
Aclo Acculoy PCA083L Polycarbonate ABS Alloy
Density 1.111 g/cc
0.04014 lb/in³
ASTM D792
Aclo Accutech Polypropylene Homopolymer HP0339M30CL Mica Reinforced Coupled