Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.111 g/cc | 0.04014 lb/in³ | ISO 1183 |
Lanxess Durethan® AC 30 DUS027 000000 Nylon 66 PA 66, non-reinforced, injection molded, impact modifiedInformation provided by LANXESS. |
|||
Density | 1.111 g/cc | 0.04014 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Density | 1.111 g/cc | 0.04014 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Density | 1.111 g/cc | 0.04014 lb/in³ | ASTM D792 |
Aclo Acculoy PCA083L Polycarbonate ABS Alloy |
|||
Density | 1.111 g/cc | 0.04014 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0339M30CL Mica Reinforced Coupled |