Suzhou Hipro Polymers Hiprolon® 90 NN Nylon 612, condition

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer Suzhou Hipro Polymers
Trade Name Hiprolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Suzhou Hipro Polymers Hiprolon® 90 NN Nylon 612, condition.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hiprolon® 90 NN is medium viscosity polyamide 6.12. Features: low density, low water absorption, high dimension stability, high impact and notched impact resistance, good chemical resistance and transparency. It is widely used as neat resin for further compounding, general injection molding and filament extrusion.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Water Absorption 1.01 %
1.01 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.0 MPa
7690 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2/1A
Tensile Modulus 1.70 GPa
247 ksi
ISO 527-1/-2
Flexural Modulus 1.80 GPa
261 ksi
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ISO 11357