Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa SINKRAL B23 ABS, Heat Stabilized  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa SINKRAL B23 ABS, Heat Stabilized  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-25 High heat resistant grade with good impact resistance. Suitable for injection moulding and extrusion (profiles).Unfilled. Suitable for Injection Molding, Profile Extrusion. Supplied as pellets. Contains lubricant and release agent.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Water Absorption 1.0 %
1.0 %
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Humidity Absorption
Melt Flow 2.7 g/10 min

@Load 10.0 kg,
Temperature 220 °C
2.7 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
50 mm/min
Elongation at Break 15 %
15 %
5 mm/min
Elongation at Yield 3.2 %
3.2 %
50 mm/min
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min
Charpy Impact Unnotched 14.0 J/cm²
66.6 ft-lb/in²
11.0 J/cm²

@Temperature -30.0 °C
52.4 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C
192 °F
Vicat Softening Point 107 °C
225 °F
50°C/hr; 50N
Glass Transition Temp, Tg 120 °C
248 °F
10°C/min test
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.7

@Frequency 100 Hz
2.7

@Frequency 100 Hz
3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
Dielectric Strength 30.0 kV/mm
762 kV/in
Dissipation Factor 0.0065

@Frequency 1e+6 Hz
0.0065

@Frequency 1e+6 Hz
0.0090

@Frequency 100 Hz
0.0090

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: