Material Notes:
Tantalum Carbide key properties: Extremely hard refractory ceramic material. The hardness is only exceeded by diamond, Very High melting point, High DensityTantalum Carbide main applications domains: High temperature protection layer against high corrosive ambient, Cutting toolsInformation provided by Acerde
Physical Properties Metric English Comments
Density 13.9 g/cc
0.502 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 9.0 - 10
9.0 - 10
Thermal Properties Metric English Comments
Melting Point 3880 °C
7020 °F