Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.95 g/cc | 0.287 lb/in³ | |
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Latrobe CSS-42L™ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness .. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Special Metals INCOLOY® A-286 Iron-Nickel-Chromium Alloy Data provided by the manufacturer, Special Metals. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Special Metals INCOLOY® Alloy 800HT™ A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | soft annealed |
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Uddeholm Vanadis 30 is a Co high alloyed powder metallurgy high speed steel corresponding to AISI M3:2 + Co. The high compressive strength, 67 HRC, and good abrasive wear resistance makes Uddeholm V.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Carlson C 800 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Carlson C 800AT Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 800AT is a modification of Carlson Alloy C 800, exhibiting higher creep and rupture strengths. This nickel-iron-chromium alloy has a carbon content restricted to .. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 35% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 48% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 52% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 60% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 70% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 90% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, Annealed Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Density | 7.95 g/cc | 0.287 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel JS700® Alloy (UNS N08700) Allegheny Ludlum's Corrosion resistant engineering alloy, JS700®, is a high-alloy, fully austenitic, superaustenitic stainless steel. This alloy is a proven problem-solver in many applications whe.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
ATI Allvac® Nickelvac® 800 & 800-H UNS N08800 & UNS N08810 Nickel Superalloy Corrosion-resistant alloy for petrochemical and food processing equipment, tubing, heat exchangers, and furnaces.Property values are for samples in the metallurgical condition: 2100°F anneal + wate.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Carlson C 800H Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Assab Steels ASP 23 Cold Work Steel ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | soft annealed condition |
Assab Steels ASP 30 Cold Work Steel ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:High wear resistanceHigh compressive strength at high hardnessGood through hardening propertiesGood toughnessGood dimensional stabi.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Crucible Steel REX® M7N High Speed Steel, AISI M7 REX M7 is molybdenum type high speed steel designed with higher carbon and vanadium to provide higher hardness after heat treatment and improved wear resistance compared to M1 steel.Information prov.. |
|||
Density | 7.94 g/cc | 0.287 lb/in³ | |
Latrobe Tatmo-VN™ ASTM M7 High Speed Steel TATMO-VN is an M7 type high speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for
many cutting tool ap.. |